Open Access
表4
铝钛复合单耳不同失效模式损伤容限分析结果
参数 | 数值 | |
宽度/mm | 74 | 74 |
传力途径 | 第一路径铝 第二路径钛 |
第一路径钛 第二路径铝 |
检查门槛值/FC | 747 956 | 1 303 083 |
检查间隔/FC | 100 438 | 54 610 |
剩余强度/MPa | 92.375 3 | 59.443 6 |
剩余强度许用值/MPa | 112.173 | 62.201 2 |
检查门槛值寿命/FC | 1 495 912 | 2 606 166 |
重复检查间隔寿命/FC | 200 876 | 109 220 |